Citation:
Pandis PK, Papaioannou S, Koukou MK, Vrachopoulos MG, Stathopoulos VN. Differential scanning calorimetry based evaluation of 3D printed {PLA} for phase change materials encapsulation or as container material of heat storage tanks. Energy Procedia [Internet]. 2019;161:429–437.